夏天的時候天氣總體來說比較的炎熱,溫度相對來說也比較高。但是有些人也會選擇在夏天的時候進(jìn)行房屋的裝修。在夏天的時候進(jìn)行房屋裝修回俐,不但對裝修工人的體力來說是一個巨大的挑戰(zhàn),甚至對裝修材料來說,能不能良好的進(jìn)行使用壶缚,也是一個很大的問題,尤其是刮膩?zhàn)佑亍D敲聪奶爝M(jìn)行裝修溉奕,膩?zhàn)臃廴菀壮霈F(xiàn)哪些問題呢褂傀?膩?zhàn)臃蹚S家的小編匯總了三個主要的問題。
In summer, the weather is generally hot and the temperature is relatively high. But some people also choose to decorate their houses in the summer. House decoration in summer is not only a great challenge to the physical strength of decoration workers, but also a big problem to the decoration materials, especially putty. So summer decoration, putty powder prone to what problems? Three main problems are summarized in the compilation of putty powder manufacturers.
濟(jì)南膩?zhàn)臃?/div>
Jinan putty powder
問題一:干得快
Problem 1: fast work
膩?zhàn)臃哿显谕袄镎{(diào)配時干的很快加勤,難施工仙辟,批刮后失水快,不能正常收壓或施工后干燥過快鳄梅。
The putty powder dries very fast when it is mixed in the bucket, so it is difficult to construct. It loses water quickly after scraping. It can't be compressed normally or dried too fast after construction.

原因:施工環(huán)境氣溫太高叠国,濕度太低、通風(fēng)太強(qiáng)及陽光直曬戴尸,膩?zhàn)又械膹?fù)合材料反應(yīng)加速粟焊。
Reasons: the temperature of construction environment is too high, the humidity is too low, the ventilation is too strong and the sunlight is direct, and the reaction of composite materials in putty is accelerated.
解決方案:預(yù)防為主,注意施工環(huán)境孙蒙,避免在高溫時段项棠、陽光直曬時段施工,控制施工場地通風(fēng)強(qiáng)度挎峦。當(dāng)基面出現(xiàn)太過干燥沾乘、 吸水快的情況時建議刷涂界面劑或者預(yù)先濕潤基面(但不能有明水)再施工。
Solution: prevention first, pay attention to the construction environment, avoid construction in high temperature period and direct sunlight period, and control the ventilation intensity of the construction site. When the base surface is too dry and absorbs water quickly, it is recommended to brush the interface agent or wet the base surface in advance (but there is no open water) before construction.
問題二:掉粉诽泪、 脫層
Problem 2: powder falling and delamination
施工完成及干透后杰赴,用手觸摸有掉粉現(xiàn)象,嚴(yán)重的甚至出現(xiàn)前后兩道膩?zhàn)又g或膩?zhàn)优c基底之間相互剝離挂闺。
After the construction is completed and dried thoroughly, there is powder dropping phenomenon when touching with hands. In serious cases, there is even peeling between the front and back putty or between the putty and the base.
原因:膩?zhàn)釉诟邷馗稍飼r施工便金,水分揮發(fā)快,沒有足夠水分進(jìn)行固化轮贫,因而容易脫粉断克。而底層膩?zhàn)邮杷煞刍瘒?yán)重,面層膩?zhàn)犹仓膈耍稍锾鞎斐擅搶右至铡A硗?外墻膩?zhàn)颖挥晁疀_刷后,粘結(jié)劑流失痊缎,重批后也容易脫層果嗜。
Reason: Putty in high temperature dry construction, moisture volatilization fast, not enough moisture for curing, so easy to powder. The bottom layer putty is loose and powdered seriously, the surface layer putty is too hard, drying too fast will cause delamination. In addition, after the external wall putty is washed by rain, the binder is lost, and it is easy to peel off after re approval.
解決方案:高溫、干燥強(qiáng)風(fēng)天氣施工石勋,更好將基面潤濕無明水后再進(jìn)行膩?zhàn)邮┕げ箍拧J┕r要收壓密實(shí),適度掌握干燥時間缓待。
Solution: high temperature, dry and windy weather construction, it is best to wet the base surface without water before putty construction. During the construction, the pressure should be collected and compacted, and the drying time should be controlled appropriately.