膩子粉經(jīng)常出現(xiàn)的問題和預防方法丰扁!
來源:http://m.bjtsdc.com 日期:2019-05-13 發(fā)布人:
膩子打磨粗
Putty polished roughly
現(xiàn)象:膩子批刮成活后秕栓,打磨砂痕粗。
Phenomenon: After the putty is scraped alive in batches, the abrasive marks are rough.
緣由:1、磨料太粗粟翔。
Reasons: 1. Abrasives are too coarse.
2桅狠、膩子被混入其它物質(zhì)。
2. Putty is mixed with other substances.
3轿秧、膩子未干中跌。
3. Putty is not dry.
4、耐水膩子枯燥太快菇篡,保濕時間短漩符,未到達正常粘結強度。
4. Water-resistant putty is too dry and fast, and its moisturizing time is too short to reach the normal bonding strength.
預防:1驱还、選用360#--600#砂紙砂磨.嗜暴。
Prevention: 1. Choose 360 # - 600 # sandpaper grinding.
2、膩子分配時只需加水.议蟆。
2. When putty is distributed, only water is needed.
3闷沥、砂磨時,膩子應干到八成以上。
3. When sanding, putty should be dried up to more than 80%.
4咪鲜、施工時應依據(jù)環(huán)境氣候適度控制膩子的枯燥時間狐赡。
4. The dry time of putty should be moderately controlled according to the environment and climate during construction.
整改:用較細砂紙修磨或上過底漆后用底漆配滑石粉刮補。
Rectification: grinding with fine sandpaper or scraping with primer and talc powder.
顏色不一
Different colors


現(xiàn)象:膩子施工后疟丙,外表有色差或色斑。
Phenomenon: After putty construction, there are color differences or spots on the surface.
緣由:1藻礁、運用了不同型號或批次的產(chǎn)品會有細微色差聋遮。
Reasons: 1. Products of different models or batches will have slight color difference.
2、基層未處置好庆率,滲色仪丛。
2. The grass-roots units are not disposed of properly and seepage.
3、膩子中混入其它物質(zhì)软殿,配比或攪拌不平均卒粮。
3. Putty mixed with other substances, the mixing ratio or stirring is uneven.
4、被污染骨惫,如噴漆钱挺,滲水,油煙等蜀勃。
4. Contaminated, such as spray paint, water seepage, soot, etc.
預防:1辣沧、壓光膩子表層應選用同型號同批次產(chǎn)品。
Prevention: 1. Calendering putty surface should choose the same model and batch products.
2驼鳞、對基層污漬必需肅清或封鎖處置哀铡,接縫王要待干透后刷耐黃變封鎖底漆。暴露金屬要做防銹處置。
2. The base stains must be cleaned up or blocked. The seam king should brush the yellowing resistant blocking primer after drying out. Exposure to metal should be treated with rust prevention.
3抒痒、施工時要留意現(xiàn)場防護幌绍。
3. Attention should be paid to site protection during construction.
整改:1. 膩子資料色差上過涂料后即可消弭。
Correction: 1. Putty material color difference can be eliminated after coating.
2. 污染性色差需肅清污染源并對受污染基層做封鎖處置故响。
2. Pollutant color difference needs to be cleaned up and blocked at the polluted grass-roots level.